›› 2018, Vol. 38 ›› Issue (7): 592-596.

• 基础研究 • 上一篇    下一篇

3D打印聚乙烯醇/纳米羟基磷灰石支架与丝素蛋白/聚乙烯醇/纳米羟基磷灰石支架的性能比较

丁刘闯1,赵小琦1,韩祥祯1,周琦琪1,宋艳艳1,张梦雪2,何惠宇3   

  1. 1. 新疆医科大学第一附属医院口腔修复科
    2. 石河子大学第一附属医院
    3. 新疆医科大学第一附属医院
  • 收稿日期:2018-01-25 修回日期:2018-03-05 出版日期:2018-07-28 发布日期:2018-07-28
  • 通讯作者: 何惠宇 E-mail:hehuiyu01@126.com
  • 作者简介:介绍信转让协议收。
  • 基金资助:
    国家自然科学基金

Performance comparison of three-dimensional printed silk fibroin/polyvinyl alcohol/nano-hydroxyapatite scaffold and polyvinyl alcohol/nano-hydroxyapatite scaffold

  • Received:2018-01-25 Revised:2018-03-05 Online:2018-07-28 Published:2018-07-28

摘要: 目的 采用3D打印技术制备3D打印聚乙烯醇 /纳米羟基磷灰石支架与丝素蛋白/聚乙烯醇/纳米羟基磷灰石支架,并对其进行表征。方法 采用3D打印技术制作聚乙烯醇/纳米羟基磷灰石支架以及丝素蛋白/聚乙烯醇/纳米羟基磷灰石复合支架。进行孔隙率、扫描电镜、压缩力学性能及细胞毒性检测。 结果 ①扫描电镜观察:丝素蛋白/聚乙烯醇/纳米羟基磷灰石支架结构规则,网状结构清晰,交通支连续,层层之间搭接良好,支架空隙均一。相同倍数下,聚乙烯醇/纳米羟基磷灰石支架网状结构连续性较差。②压缩力学性能:相同应力情况下(10 MPa),3D打印丝素蛋白/聚乙烯醇/纳米羟基磷灰石支架的应变大于3D打印聚乙烯醇/纳米羟基磷灰石支架。③孔隙率:3D打印丝素蛋白/聚乙烯醇/纳米羟基磷灰石支架的孔隙率大于3D打印聚乙烯醇/纳米羟基磷灰石支架。④细胞毒性检测:不同时间点两组支架的细胞增殖率无明显差别。结论 结果表明:3D打印聚乙烯醇 /纳米羟基磷灰石支架与丝素蛋白/聚乙烯醇/纳米羟基磷灰石支架具有良好的理化性能和细胞相容性。

关键词: 丝素蛋白, 3D打印, 纳米羟基磷灰石

Abstract: Objective  To prepare silk fibroin(SF)/polyvinyl alcohol(PVA) / nano-hydroxyapatite (nHA) scaffold and polyvinyl alcohol(PVA) / nano-hydroxyapatite (nHA) scaffold using 3D printing technology and detect their performances. Methods 3D printing technology was used to print SF/PVA/nHA scaffold and PVA/nHA scaffold. Porosity, morphology, mechanical properties and cytotoxicity of different scaffolds were detected. Results  ①Under scanning electron microscope, SF/PVA/nHA scaffold had regular scaffold structure and clear network structure, exhibited continuous communicating branch, well-connected overlap joint, and uniform scaffold space. Under the same multiples, the network structure continuity of PVA/nHA scaffold was poorer. ②Compressive mechanical properties: Under the same stress(10 Mpa), the strain of SF/PVA/nHA scaffold was larger than that of PVA/nHA scaffold. ③The pore size of group SF/PVA/nHA scaffold was significantly larger than PVA/nHA scaffold. ④Cell toxicity detection: The deformation of SF/PVA/nHA scaffold ,under the same stress(10 MPa),was larger than PVA/nHA scaffold. There was no significant difference in cell appreciation rate between two groups of scaffolds at different time points. Conclusions 3D printing SF/PVA/nHA scaffold and PVA/nHA scaffold hold good physicochemical performance and cytocompatibility.

Key words: silk fibroin solution, 3D printing, nano-hydroxyapatite