2种耐湿性托槽粘结体系粘结强度的比较研究

柳杨,韩翔   

  1. 杭州市萧山区第一人民医院
  • 收稿日期:2012-06-26 修回日期:2012-08-16 出版日期:2013-05-28 发布日期:2013-06-20
  • 通讯作者: 柳杨 E-mail:liuyang0824@hotmail.com

Comparison of bond strength between two moisture resistant bracket bonding system

  • Received:2012-06-26 Revised:2012-08-16 Online:2013-05-28 Published:2013-06-20

摘要: 目的 比较3M Transbond MIP处理液+3M Transbond PLUS变色光固化粘结剂与GC Ortho LC光固化树脂加强型玻璃离子2种粘结体系的粘结强度。方法 收集因正畸治疗而拔除的上颌前磨牙80颗,按照随机化原则分成8组,每组10颗。将2种粘结体系分别在干燥、水分污染、唾液污染和血液污染的条件下完成托槽粘结,用电子万能试验机测试剪切强度,并在显微镜下用ARI指数评价各组牙齿表面残余的粘结剂。 结果 在剪切强度测试中,第1组与第5组比较,第2组与第6组比较,第3组与第7组比较,P>0.01,均无统计学差异;第4组与第8组比较,P<0.01,有统计学差异。ARI评分结果提示两者在干燥、水分污染及唾液污染环境下的ARI平均分值无统计学差异,但在血液污染的条件下,GC Ortho LC的ARI值明显降低。结论 3M Transbond MIP处理液+3M Transbond PLUS变色光固化粘结剂与GC Ortho LC光固化树脂加强型玻璃离子在干燥、水分污染及唾液污染的环境下,粘结强度无明显差异,在血液污染的条件下,推荐使用3M Transbond MIP粘结体系。

关键词: 3M Transbond MIP处理液, GC Ortho LC, 粘结强度, 剪切强度, ARI, 3M Transbond MIP primer, GC Ortho LC, bond strength, shear bond strength, ARI

Abstract: Objective To compare bond strengh of 3M Transbond MIP primer+3 M Transbond PLUS discolor light curing adhesive and GC Ortho LC light-cured resin-reinforced glass ionomer. Methods The study consisted of 80 maxillary premolars which were extracted for orthodontic treatment.The teeth were randomly divided into 8 groups, with 10 specimens in each.The specimens were bonded with brackets with the two bonding systems under the conditions of dryness, water pollution, saliva contamination and blood contamination respecitively. The shear bond strengh of each tooth was done with electronic universal testing machine, and the ARI scores were used to evaluate the residual adhesive on surfaces of teeth in each group under the microscope. Results In the shear bond strength test, comparing the first group with the fifth group, the second group with the sixth group, the third group with the seventh group, P>0.01,there was no statistically significant difference; comparing the fourth group with the eighth group, P<0.01, there was statistically significant difference. The results of ARI showed that there was no statistically significant difference in average ARI scores between the two bonding systems under the conditions of dryness, water pollution,and saliva contamination, but under blood contamination, the ARI score of GC Ortho LC decreased significantly. Conclusion Under the conditions of dryness, water pollution, and saliva contamination, the shear bond strength of 3M Transbond MIP primer+3 M Transbond PLUS discolor light curing adhesive and GC Ortho LC show no significant difference, but under blood contamination, we recommend using 3M Transbond MIP primer+3 M Transbond PLUS discolor light curing adhesive.